I would like to know if for a produced water injection: pumping temperature: 120°F to 160 max
TDS: 3500mg - 25000 mg
Chloride concentration : >100ppm
Viscosity: 1.3
Density : 1.004 à 1.01
The choice with a cast casing in A 216WCB with internals ( impeller, shaft, rings..)in 13%Cr is correct, or if its better to choose a cast casing in 13% Cr with internals in 13%Cr?
Thank you for your help
JLuc
TDS: 3500mg - 25000 mg
Chloride concentration : >100ppm
Viscosity: 1.3
Density : 1.004 à 1.01
The choice with a cast casing in A 216WCB with internals ( impeller, shaft, rings..)in 13%Cr is correct, or if its better to choose a cast casing in 13% Cr with internals in 13%Cr?
Thank you for your help
JLuc