I am needing to clean and passivate some significant quantities of 316 s/s on an offshore platform in the Timor Sea. The usual HF and HNO3 based pickling pastes are considered too hazardous and environmentally unfriendly to use and wash overboard. I believe there may be a citric based product which may be useful for mild levels of contamination after removal of contaminated areas with a flapper wheel or wire brush. Can anyone please advise the name of a commercially available and environmentally friendly product?
 
"CitriSurf is an environmentally friendly citric acid based cleaner and passivation product for use with all grades of stainless steel. CitriSurf replaces hazardous Nitric Acid products, and meets ASTM A-967."
Both gel and immersion versions.
Contact: Lee Kremer
E-mail: Kremer@CitriSurf.com
Phone (847) 854-2800
Fax (847) 854-2830
 
Thankyou one and all. I will follow up those suggestions
 