Hy all
Q :I have a P8-P8 PQR produced on a SA 312-304L-304L base material with a ER308L filler wire.
I want to qualify a WPS of 316L-316L with ER316L F no,A no and SFA no are all the same.
Do I need to requalify my PQR in this instance or can i use the same PQR....
Regards
Tman