Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Equivalent ASME material

Status
Not open for further replies.

jerin james

Mechanical
Sep 17, 2020
30
Dear Sirs,

Can you please advise the equivalent ASME UNS grade for below materials :

CuZn28Sn3
CuZn38SnA1
CuZnA1

Tried finding on google but couldn't trace out.

Thanking you
Jerin
 
Replies continue below

Recommended for you

Do you have any info? A Spec? A product form? A Tradename?
I can guess, but that isn't what you want.


= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
The only thing I have found in the ASME Code is in ASME Section II Part B, SB-171 which covers CuZn38Sn1.

I didn't find anything regarding the two others. May be they aren't approve.
 
Go to Copper.org ans search there. The CDA has all things copper based.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
Edstainless,

The product form is tube.I found these material on 1970's tube bundle drawings.
Thanks
 
And it is a European drawing? You may have to go back to an old version of the code for some of these materials.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
@EdStainless,

Yes, the drawings were preapred by a fabricator in England and later tube bundle was replaced by a german fabricator.
Jerin
 
@jerin james

In my opinion, the nearest equivalent your materials are following this:
- CuZn28Sn3 : ASME SB 111 C4 series (C44300 / C44400 / C44500
- CuZn38SnA1 : ASME SB 111 C2 series (C23000 / C28000)
- CuZnA1 : ASME SB 111 C6 series (C60800 / C61300 / C61400 / C68700

Thanks
Tito F, YT Channel "FN Engineering"
 