Dear Sirs,

Can you please advise the equivalent ASME UNS grade for below materials :

CuZn28Sn3
CuZn38SnA1
CuZnA1

Tried finding on google but couldn't trace out.

Thanking you
Jerin
 
Do you have any info? A Spec? A product form? A Tradename?
I can guess, but that isn't what you want.


= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
The only thing I have found in the ASME Code is in ASME Section II Part B, SB-171 which covers CuZn38Sn1.

I didn't find anything regarding the two others. May be they aren't approve.
 
Go to Copper.org ans search there. The CDA has all things copper based.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
Edstainless,

The product form is tube.I found these material on 1970's tube bundle drawings.
Thanks
 
@IdanPV & @0707, thank you so much your replies.
 
And it is a European drawing? You may have to go back to an old version of the code for some of these materials.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
@EdStainless,

Yes, the drawings were preapred by a fabricator in England and later tube bundle was replaced by a german fabricator.
Jerin
 
@jerin james

In my opinion, the nearest equivalent your materials are following this:
- CuZn28Sn3 : ASME SB 111 C4 series (C44300 / C44400 / C44500
- CuZn38SnA1 : ASME SB 111 C2 series (C23000 / C28000)
- CuZnA1 : ASME SB 111 C6 series (C60800 / C61300 / C61400 / C68700

Thanks