looking for an equivalant to SAE J1392 or G40.21-44W
 
Replies continue below

Recommended for you

SAE J1392 is now obsolete and has been replaced by SAE J2340. SAE J2340 uses only SI units, so 050X according to J1392 is now called 340X in J2340. ASTM A1008 (cold rolled) and ASTM A1011 (hot rolled) also specify HSLA steels in sheet/coil form.
 