Good morning,
In terms of bs7671 does anyone know if EPR insulated cables fall under thermosetting or thermoplastic in the appendix tables?

Thanks
 
It's a thermosetting cable. Haven't got my copy of the Big Blue Book to say exactly which table applies. :-)
 