Dear friends,

I am looking for the service temperatures of the both.

I would like to use one of them as a material for heat shield.

Can anyone refer me source or where can I look for this information?

Thanks.
 
Replies continue below

Recommended for you

Depending on the grade and cure system used EPDM is good for temperatures up to around 100°C. This will apply to the blend with PP too.

forumtowers.com
 
Thanks, I do not know the grades for both.

Where can I find a source to look for?

Actually, it would be good if I can find data to compare EPDM+PP and EPDM ..
 