Hi, i'm currently working on an incident regarding some engine radiator EPDM gaskets about 722 overall length and 3mm section
There is a small batch of 32 pieces which supposedly left manufacturing plant within length specification but when arrived to to assembly plat (radiator assembly) they were measured on a go nogo gage and resulted to be about 3mm longer than upper specification
im launching the next actions
- Packaging tests with lower and higher material density per box
- Thermally validate autoclave operation
what wold the causes be to get the gaskets stretched?
Can you share some information regardig how curing affect gasket length?
I Really appreciate your comments
There is a small batch of 32 pieces which supposedly left manufacturing plant within length specification but when arrived to to assembly plat (radiator assembly) they were measured on a go nogo gage and resulted to be about 3mm longer than upper specification
im launching the next actions
- Packaging tests with lower and higher material density per box
- Thermally validate autoclave operation
what wold the causes be to get the gaskets stretched?
Can you share some information regardig how curing affect gasket length?
I Really appreciate your comments