As far as I know, there should be no entrained air in interior SOG & concrete on metal deck, because none shall be exposed to freeze-thaw. And of either of these floors are to be trowel finished then the entrapped air is to be no more then 3%.
Is my understanding correct or is it too simplistic?
Thanks.