Is there a symbol to callout end returns? Or are end returns called out with a note in the tail?

Faith is taking the first step even when you can't see the whole staircase. -MLK
 
Replies continue below

Recommended for you

Recently, I have been using a second weld annotation pointing to the return edges, but in the past have called out in the tail as you mention. I don't think it matters as long as they know that they have to precisely provide the return weld, no more, no less.

I also have a general note about not over-welding returns, etc.

"It is imperative Cunth doesn't get his hands on those codes."
 