EN S355N - US grade equivalent

Status
Not open for further replies.

Tagger

Mechanical
Joined
Aug 10, 2001
Messages
47
Location
US
What is the US grade equivalent to EN S355N material.
We have an ASM 'Worldwide Guide To Equivalent Irons and Steels' 3rd edition, and I could not find it. For the future where can you find equivalents for this EN series?
 
Thanks for the help. It says on the drawing to Manganese Phosphatize the material. Is that some hardening process?
Is the material received that way for machining, or is it done after machining? How do you specify it to whomever? Do you just say I need this manganese phosphatized, or do you get more specific (like case depths, Rc, etc.)?
 
S355N is normalised , fine grain structural steel per EN 10113-2. Is for low temperature application. No real equivalent in ASTM , but close to A 808
 
I found the material thanks to the site kenvlach linked me to. It cross referenced to a E36-3 France which is a High-Mn 1513 carbon steel.
 
Also I figured out what Mn-Ptize is. Basically it is a conversion coating to help prevent corrosion, galling, etc. It chemically converts the surface of the metal. I take it this process needs to be done after machining the part?
 
Yes, the phosphating operation needs to take place after machining. Phosphating is very common pre-treatment, with iron phosphate, zinc phosphate, and manganese phosphate all used for different purposes. You should obtain more information about the Mn phosphating. Specifically, what coating weight is needed? Is the phosphate supposed to be subsequently oiled?
 