Is there an equivalent cast material in the EN specs to ASTM A747 CB7Cu-1?

Thanks
 
Replies continue below

Recommended for you

I'm not sure the EN specification, but the German Standard would be: DIN SEW 410 - grade: GX5CrNiMo165
 
The designation is GX5CrNiCu16-4 (1.4525) according to EN 10283.
 
Thanks to all. The matter has now been resolved.
 