Hello,

I have encountered a problem when calculating the allowable stresses for bolts made of A2-70 material.
In a formula 5.2.2-1 of EN 13480-3 it is stated to use the second formula if Rm,t is available.

For temperature of 20 °C the ff value is determined acc. to the second formula, becauseRmt is known for 20°C.
This leads to higher allowable stresses at higher temperatures, because Rmt is not known and the value is calculated according to the first formula.
For example, allowable stress at 35 °C is much higher than allow. at 20°.

Has anyone approached this problem before and what would be the advice on how to proceed?

Thank you for your time!

Kind Regards,
Tomislav Begic
 
Replies continue below

Recommended for you

Is this for a standard flange? Have you looked at para 6.6.3 for that matter? That refers to EN 1515 series.

Huub
- You never get what you expect, you only get what you inspect.
 

I'd expect the tensile stress @20 °C and @ 35 °C to be almost the same. In any case the formulas reported in EN 13480-3 refer to Rp,1.0 and not Rp,0.2.

As suggested by XL83NL, you could take a look to EN 15515-4, which as standard reference for X5CrNi18-10 (EN 1.4301EN) addresses to EN 10269, where you can find mechanical properties vs temperature tables.

 