EN 10213 Impact testing

Status
Not open for further replies.

bruv

Materials
Feb 19, 2002
239
EN10213:2003 requires impact testing for a number of material grades. Section 7.2.2.1 says that "mechanical properties shall conform to the values given in Table 4 for ferritic & martensitic grades".

Referring to Table 4, (alloy number 1.7379, equivalent to ASTM A217 WC9), it just says "Impact test KV, 40J min". Should this value be interpreted as a minimum average, or minimum individual reading?

Normally this would not be an issue, as most specifications state both, but what happens if your results are, for example 37J, 48J, 47J, average 44J?
 
Replies continue below

Recommended for you

My interpretation of 7.2.2.1 and Table 4 are minimum individual readings, but I have never actually purchased/specified anything according to this standard.
 