I'm hoping to finalize a design for a precast pea gravel concrete wall panel to serve as a stay in place form for cast in place concrete. It will be a non braced system to hopefully contain form pressure of 1500 psf at the bottom of a ten foot pour. My concern is that the embedded expanded steel along with concrete displacement created by styrofoam embedment will be strong enough. I have worked out equations setting shear strength at 2 x sqrt 4000 x bo (perimeter) x d (depth). Since the panels will be stacked vertically, there will be compressive force which according to eqn (11-4) may increase the multiplier two to three. Any thoughts or clever ideas would be greatly appreciated. Would glass or steel fiber (Helix) be a no brainer addition?

24_iso_back_chamfer_inside_xrfmpe.jpg


cross_section_horizontal_ea8zw8.jpg


dimensions_zwypcp.jpg


bearing_load_formula_nz11fa.png


scaffold_slab_support_g9gpti.jpg


shear_strength_equation11-3-2_n5qve8.png


side_view_dimensions_pimlsr.jpg


pulloutl_xtsom4.jpg


initial_pullout_ibwzn4.jpg


Looking at first smaller pull out area affecting larger panel intersection.

panel_face_reaction_z1avo0.jpg
 
Replies continue below

Recommended for you

PVA fiber or helix steel fiber could be added to the panel mix. I've used with approval Helix fiber as a substantial rebar replacement in the cast in place, at 13 pounds per cubic yard.
 