Despite chemistry being OK, we experience poor elongation in our plain carbon steels and low alloy steel castings (stainless is OK).
IE. 4140 normalized 4% - 5% annealed 8% - 10%
Can get higher elongations, but on the expense of Tensile and Yield strengths.
Melting - coreless induction furnace. Steel is deoxidized by ladle addition of .02% Al and .05%Ti.
Thank you