Elimination of a cladding part to create a bevel 3

Status
Not open for further replies.

ATsampalas

Materials
Joined
Feb 26, 2004
Messages
43
Location
BE
thread725-146231
I am trying to find the precise English word of "the elimination of a cladding part to create a bevel" (see attached figure).
Justification of this operation :
a)Welding (carbon products) base metal 1+2
b)Appropriation (cleaning, machining or grinding) of the surface before CND
c) CND
d) Welding (cladding side) with stainless products...
Sincerely,
A_Tsampalas
 
ATsampalas, not sure what the formal term is, if any, but I think "strip" or "remove cladding for XX distance from weld bevel" will be clear enough.

Regards,

Mike
 
Agree with SnTMan and use a note or the phrase "locally remove the cladding from the weld region as indicated"
 
Very like SnTMan, we used "strip back cladding" a minimum of X-inch from weld bevel in our specifications.

 