Yes , vastly different melting temps
These work in Ultra high vacuum and 1000C
What Im doing is joining SS to tantalum pretty well , It must be a braze
In 20% of parts I get cracking and the SS, just a does not join to the Ta ,
I dont know why
Its not a metallurgy problem , just a how lucky I get trying to seal SS to Ta, not too cool and not too hot