Hallo to everybody !
Please, I’d like to know if somebody can help me in this issue:
When I consider the galvanic couple of
1) aluminum and copper, the electrode potential of aluminum is -1.66V, while copper is +0.34V.
As a consequence aluminum is the less noble metal and will be subjected to corrosion.
2) copper and silver. Copper +0.34V Silver 0.80. Therefore copper will be corroded
3) Copper and Tin. Copper +0.34V, Tin +0.1335V. Tin will be corroded
4) Aluminum with silver or tin = > aluminum will be corroded anyhow.
Let’s consider that all of these reactions are in the same environment.
Question 1: Is there a relationship between the potential difference and the kinetics of corrosion ? Ex: higher the potential difference, faster the corrosion
Question 2: If there is, which is this relation ?
Question 3: is the corrosion affected also by the quantity of the two materials ? Ex: in case 1, should the aluminum be present in a small quantity, the quantity will disappear in a shorted time that a bigger one, shouldn’t it ?
Thanks in advance !
Please, I’d like to know if somebody can help me in this issue:
When I consider the galvanic couple of
1) aluminum and copper, the electrode potential of aluminum is -1.66V, while copper is +0.34V.
As a consequence aluminum is the less noble metal and will be subjected to corrosion.
2) copper and silver. Copper +0.34V Silver 0.80. Therefore copper will be corroded
3) Copper and Tin. Copper +0.34V, Tin +0.1335V. Tin will be corroded
4) Aluminum with silver or tin = > aluminum will be corroded anyhow.
Let’s consider that all of these reactions are in the same environment.
Question 1: Is there a relationship between the potential difference and the kinetics of corrosion ? Ex: higher the potential difference, faster the corrosion
Question 2: If there is, which is this relation ?
Question 3: is the corrosion affected also by the quantity of the two materials ? Ex: in case 1, should the aluminum be present in a small quantity, the quantity will disappear in a shorted time that a bigger one, shouldn’t it ?
Thanks in advance !