sensiblesteve
Mechanical
I'm caught up on a material for a latching configuration.
I've been hours on Matweb and the best I can come up with is a 304/L - 60% elongation @ yeild - Youngs @ 28000 ksi.
Am I on the right track.
I need a 1/4" deflection with as little as possible deformation. 1 cycle.[the configuration is much like a backpack clip]
Any input would be greatly appreciated.
Thank you,
Steve Scott
I've been hours on Matweb and the best I can come up with is a 304/L - 60% elongation @ yeild - Youngs @ 28000 ksi.
Am I on the right track.
I need a 1/4" deflection with as little as possible deformation. 1 cycle.[the configuration is much like a backpack clip]
Any input would be greatly appreciated.
Thank you,
Steve Scott