arbitrader
Mechanical
I have to demonstrate to NJDEP that styrene monomer and methylene chloride do not have a destructive effect on concrete.
The Portland Cement Association has a document that lists the effects from a limited list of chemicals but unfortunately the aformentioned two are not listed.
Can anyone shed any light on a reference or test method to test the destructive effect?
The Portland Cement Association has a document that lists the effects from a limited list of chemicals but unfortunately the aformentioned two are not listed.
Can anyone shed any light on a reference or test method to test the destructive effect?