What kind of effect will a pH drop in RO product water have on regular black iron pipe used to move 125 psi steam?
The original pH was 6.5. It's dropped to 5.4 - 5.7.
Would this much of a pH drop accelerate the rusting/breakdown of black iron pipe used to move regular cold water?
The original pH was 6.5. It's dropped to 5.4 - 5.7.
Would this much of a pH drop accelerate the rusting/breakdown of black iron pipe used to move regular cold water?