Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations KootK on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Effect of Aging in Losses of Transformers and Conductors

Status
Not open for further replies.

CKent

Electrical
Aug 27, 2003
42
How does the aging of power system equipments, such as power transformers and conductors, affect its loss? Are there any correlation between age and loss?
 
Replies continue below

Recommended for you

Just two comments of possible aging mechanisms to increase loss. I’m not sure how common these are.

Vibration can abrade the core interlaminar insulation and increase core loss.

Heat transfer surfaces can get fouled, resulting in higher temperature (for a given load), resulting in slight increase in conductor resistance (approx 0.4% per degree C) and resistive losses.

=====================================
Eng-tips forums: The best place on the web for engineering discussions.
 
Aging affects insulation mainly, not the conductor itself. Except for the possible minor effects noted by Pete, I would not expect an increase in losses with age. Age does not increase the resistance of a conductor.
 
The dielectric loss of the transformer insulation may increase with aging. But in the overall scheme of very low trafo losses (1 to 2 %), this is a very minor bee sting.

Copper and iron losses do not increase with aging.
 