Can anyone give me a rough method of calculating eddy current losses?
Here's the situation:
I have a high current conductor (10kA-20kA) bolted to a chunk of stainless which is enventually insulated. How can I make a rough estimate for eddy current losses in the stainless?
The stainless is 304 with roughly the following properties:
Resistivity - .000072 ohm-cm
Permeability - 1.008
The copper is rectangular water cooled with the following dimensions:
approx 3 3/8" by 6 1/2"
Here's the situation:
I have a high current conductor (10kA-20kA) bolted to a chunk of stainless which is enventually insulated. How can I make a rough estimate for eddy current losses in the stainless?
The stainless is 304 with roughly the following properties:
Resistivity - .000072 ohm-cm
Permeability - 1.008
The copper is rectangular water cooled with the following dimensions:
approx 3 3/8" by 6 1/2"