Hi All,

The footing size is (1.4 x 1.75)m (Fig. attached) & the SBC is 110 kN/m2

I get e> L/6 condition, Hence, I applied the 2P/BL' to calculate pressure max;
where L' is the bearing length = 3* (0.5L-e)

Thus, Qu = 2P/BL' = 102.6 kNm2

L' = 1.55 m ; P = 111.6 kN(Factored, Calculated) ;
M = 39.856 kNm (Factored, Calculated)
L = 1.75 m ; e = 0.357 m


How do I calculate moment for reinforcement from this triangular pressure profile ?
In report i found that Moment is 4.62 kNm. But I could not get the same.
Thank you.

BW-Section_dkyi7d.png
 
Also, I think it is important to check and design for the construction case, which may govern the flexural design (especially bottom of slab).

Loadings - Weight of wall + Weight of slab + Wind (in both directions)
 
I think I found mistake in the report.

When sum moment about center of the base, they included the wind (M=24.91), but forgot moment caused by the wall (P=42.3).
With the arm from center of wall to center of the base x = 0.725, for un-factored load case MCL = 24.91 + 42.3*0.725 = 24.91 + 30.67 = 55.8 (24.91 reported), P = 89.47 (ignore w4), e = 55.8/89.47 = 0.624m >> 0.27m (0.27mm in report)

For factored load case:

Pu = 1.2*89.47 = 107.36
Mu = 1.2*24.91+1.6*30.67 = 78.96 (39.856 reported)
e = 78.96/107.36 = 0.736m > distance x = 0.725m ----> Resultant force near outer wall face

Check my calculation, see if there is mistake.
 

Yes. The moment caused by the wall shall be included too due to eccentricity.
P/A + M/Z = 114.36 kN/m2 that exceeds the allowable bearing pressure (110 kN/m2) now. Subsequently, all the following design steps shall be revised. Shear check is not done.
This project'd executed long back ago.can't be revised. But I will revise my cals for my self study and will include shear check also.

And regarding the moment calculation, thank you so much for the detailed way of explaining. I am clear now. :) so, the query started with moment calculation. But I learned the concepts well now by all answers, especially you. Thank you so much :)
 
Actually, there is no need to check shear, since the wall possess the heaviest weight. But don't forget the step in your next assignment.

A simple sketch can tell thousand words, reminder of our own task/act, and easier for anybody else to understand.

At this junction, If I am you, I'll discuss with a close higher up to seek advice and direction. Usually a thorough evaluation is required. Good luck.
 
I dn't know how do they react, if I notify the missing cals of moment caused by wall. Seniors are not very approachable.
Thank you retired13 for the wishes.
 
Yes, I understand, this is a difficult situation for a new hire. I might consider send my direct supervisor an email with the finding stated. I don't know how the company will react, but you shall be safe if you don't talk too much about this incident. Keep looking for other better opportunity though. A good company shouldn't let this happen.
 
True..Thanks Again :)
 
Dear All,

This is regarding the concrete column to concrete wall panel connections that to be established by L-angle (weld). For the same structure that're discussed in this tread require this connection. Both column and wall panel are precast members. I would require to check whether this connection shown in this attached Fig. is adequate or not.


wall_f6yany.png



ele_jgf7vr.png



plan_gywprg.png



I would require to check whether this connection shown in this attached Fig. is adequate or not.

Thank you
 
Akshikas,

It is better to open a new thread, this thread is too long for people to browse. Unless you need to reference back to the calculation.
 
Dear retired13,

Posted as new thread Link. Thank you.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top