Hi Everyone,

Is there anyone that knows where or how I can find the value of heat transfer in metric if possible for
DZR Brass?

Thanks in advance.

Regards
 
Replies continue below

Recommended for you

For Admiralty brasses thermal conductivity is 111 W/(m K) at 20 °C
 