508
Nice article from Hot Rod Network I thought others might enjoy. Below are their dyno results using factory gapped, file gapped, and gapless rings.

Factory Gap:
Peak HP: 434.7 hp @ 5,700 RPM
Peak Torque: 450 lb-ft @ 4,400 RPM
Average HP (3,000-6,000 rpm): 363.3 HP
Average Torque (3,000-6,000 rpm): 425.6 lb-ft

Filed Gap:
Peak HP: 441 hp @ 5,700 RPM
Peak Torque: 459.2 lb-ft @ 4,500 RPM
Average HP (3,000-6,000 RPM): 370 hp
Average Torque (3,000-6,000 RPM): 433.9 lb-ft

Gapless:
Peak HP: 451 hp @ 5,600 RPM
Peak Torque: 465 lb-ft @ 4,500 RPM
Average HP (3,000-6,000 RPM): 375 HP
Average Torque (3,000-6,000 RPM): 440 lb-ft
 
Replies continue below

Recommended for you

Looks to all be within standard variability.
 
Interesting, but an A-B-A test sequence for each ring type would sure have been nice.

These ring gap test results on pages 1 and 2 originally appeared along with a cool graph in a document from Speed-Pro back when the parent company Sealed Power was on its own, and a premium product.
 
Have you tried measuring the ring friction in a motored test, or even a pull through test (ie put a piston in a cylinder and push on it?

Cheers

Greg Locock


New here? Try reading these, they might help FAQ731-376
 
GregLocock, I'm not sure to whom your question is directed. If it was me, the answer is no, not yet. I'm still trying to decide which ring type to use.
 
Rod, I know they call them that, the comment wasn't to you.
 
Yes, it's standard in a magazine test, the advertiser's product always produces the most power

In production engine quantity, piston rings are an ant-shit cost component. If the Total Seal Gapless were actually worth 3.5% additional horsepower and torque, they'd be universally used.
 