BACKGROUND: I am enhancing a proprietary moldless casting machine that centrifugally casts a near-perfect coating on a curved surface. The degree of perfection inversely depends on the variation in angular velocity. A servo motor drives the unit through a 100-to-1 gear speed reducer.

PROBLEM: Backlash in the gearing prevents the servo drive from maintaining a constant angular velocity.

PROPOSED SOLUTION: Provide a relatively small amount of parasitic torque in the form of a brake such that backlash is eliminated in the gearing.

NEW PROBLEM: After trying several styles of strap brakes, I've eliminated brake squeal by using a 3-1/2" 410 SS disc brake and a bicycle caliper. The current problem is DUST - this contaminates the surface of my cast workpiece. I've tried several commercial forms of disc pad compounds including Ceramic-Carbon Sintered pads which I incorrectly believed was dust free.

SOLUTION NEEDED: What type of brake pad material will emit the minimum of dust? And just as importantly, where do I get this material? I've tried the pads available from the caliper manufacture and they are VERY dusty.

Thanks in advance for your kind reply!

S.D.

 
You need to stop looking at the friction materials used for vehicles - they are designed to behave just as you describe.

You can look at metallic parts, but there will be higher noise and vibration. You may need to provide a lubricant at the surface, and you may need to provide cooling for the part.

Perhaps you can work on isolating the braking system from the casting chamber. How about a vacuum or forced air system?

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
I'm with Rod.

An electric field.

Look at engine dynos that use water brakes or eddy current brakes.

Regards

eng-tips, by professional engineers for professional engineers
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top