Duplex Stainless Steel Pickling after Welding

Status
Not open for further replies.

WeldGk

Materials
Aug 14, 2007
42
Does anyone have any information on where I can find specific information about pickling vs not pickling 2205 duplex after welding?
 
Replies continue below

Recommended for you

There is a similar document available on the Outokumpu web site.
Depending on the shield gases that you use in welding, the un-pickled welds can range from only a little worse to very bad.

= = = = = = = = = = = = = = = = = = = =