we are currently working on a new specification for Duplex SS (2205) for our site in Germany.
API 938-C recommends that base metal and welds are tested to ASTM 923 Method B or C (C is the corrosion test with ferric chloride solution).
According to German regulations VdTÜV 418 the EN ISO 3651-2 Test C (sulfuric Acid and ferric sulfate) is mandatory.
The Tests use diffeent solutions and have different acceptnace criteria (cracking vs. mass loss), nevertheless both try to identify if intermetallic phases are present.
As we would rather not specify 2 corrosion tests the question is if there is experience with only using the EN ISO test to determine corrosion resistance?
do you know of a study to compare results?
Thank you for your help!
Daniel Breyer
Inspection Engineer
we are currently working on a new specification for Duplex SS (2205) for our site in Germany.
API 938-C recommends that base metal and welds are tested to ASTM 923 Method B or C (C is the corrosion test with ferric chloride solution).
According to German regulations VdTÜV 418 the EN ISO 3651-2 Test C (sulfuric Acid and ferric sulfate) is mandatory.
The Tests use diffeent solutions and have different acceptnace criteria (cracking vs. mass loss), nevertheless both try to identify if intermetallic phases are present.
As we would rather not specify 2 corrosion tests the question is if there is experience with only using the EN ISO test to determine corrosion resistance?
do you know of a study to compare results?
Thank you for your help!
Daniel Breyer
Inspection Engineer