Hi All,
I was wondering if anyone could give some advice on a potential component issue I have which is made from UNS S32760. Basically I have a component that will be part of a subsea manifold consisting of several intricate parts and contains multiple small gaps and sealing faces. The component itself will be connected to a portion of the manifold which has a max working temp of 40 deg C, but is situated next to pipe work that has fluid passing through it at a max temp of 120 deg C. My question is will crevice corrosion be the most likely form corrosion? Are these temperatures of any concern to Super Duplex and should another material be possibly considered?
I was wondering if anyone could give some advice on a potential component issue I have which is made from UNS S32760. Basically I have a component that will be part of a subsea manifold consisting of several intricate parts and contains multiple small gaps and sealing faces. The component itself will be connected to a portion of the manifold which has a max working temp of 40 deg C, but is situated next to pipe work that has fluid passing through it at a max temp of 120 deg C. My question is will crevice corrosion be the most likely form corrosion? Are these temperatures of any concern to Super Duplex and should another material be possibly considered?