Hi,
We're using a PQR qualified with seamless pipe in duplex (S31803) : P10h-P10H. Our customer doesn't agree that we use this PQR to weld a pipe of duplex to a casting of the same grade (ASTM A890 gr 4A). The reason is that duplex casting has no P-number, so it should be separately qualified according asme IX.
If we follow strictely the code it is right. But, duplex casting has the same composition to forge or pipe duplex. Is there really a technical justification to have not assigne a P-number to duplex casting or is it just because AMSE is not an exhaustiv list and some judgment need to be taken.
thanks
Erick21
We're using a PQR qualified with seamless pipe in duplex (S31803) : P10h-P10H. Our customer doesn't agree that we use this PQR to weld a pipe of duplex to a casting of the same grade (ASTM A890 gr 4A). The reason is that duplex casting has no P-number, so it should be separately qualified according asme IX.
If we follow strictely the code it is right. But, duplex casting has the same composition to forge or pipe duplex. Is there really a technical justification to have not assigne a P-number to duplex casting or is it just because AMSE is not an exhaustiv list and some judgment need to be taken.
thanks