I am repairing a tube leak and ended up having some of the dummy or spacer tubes removed in our reheat section. I was woundering why are they there is it to support the bundle or to reduce convection. Any help would be of benifit.
Thanks
 
Replies continue below

Recommended for you

sometimes there is installed a squashed tube to maintain spacing between elements and also to reduce vibration potential.

Also, if there is found to be a lot of steam in the fluegas after you restart, it probably was not a dummy tube that you removed.
 
Dummy tube and I assume these are not connected to the reheat tube circuit are in place to maintain tube spacing to keep a uniform flue gas flow over the tube bank. Removal may cause a problem with poor performance of the boiler if the reheat tubes become miss aligned.