Does anyone have a recommendation for a barrier fluid to be used in a dual seal that will be in an anhydrous, gaseous hydrofluoric acid environment? I would like to use Fluorolube, but it causes significant swell in Kalrez orings. The engineer who had this project previous to me tried to use a Royal Purple (RP) product and according to John Crane the RP caused a slip-stick situation that caused the seal to fail. Any assistance would be appreciated.
 
What I am really interested in is what are other people using as a barrier fluid for dual seals in an anhydrous HF environment.
 
RP is usually highly recommended by Crane and the other seal mfgs... Slip stick is usually caused when a highly viscous fluid is between the faces.
 
Royal Purple (FDA grade) is a good barrier fluid.

Is your seal a dual bellows seal?
Are you getting slip stick from lack of damping on a bellows I wonder?


-
Milkboy
 
In conjunction with the Plan 52, 53, or 54, most often you will find a Plan 32 with Alkylate or Isobutane to help keep high concentrations of HF from getting near the seal. I think I've seen Isobutane used as the barrier/buffer fluid.

A lot of people are migrating to Nitrogen buffer systems with dry running or lift-off containment seals or outright to dual gas seals. This decreases worries about iron fluorides contaminating the buffer fluid as well as contamination from the flare header.

 
Using Total Seriola 22 heat transfer oil at the moment but not entirely happy with it. I am also considering using Alkylate
 