Oct 13, 2003 #1 Elroyjet Automotive Joined Sep 8, 2003 Messages 4 Location US Hay, I am working on a paint project for steel driveshafts. The question is if the part sees a 300F oven for 17 minutes, and the part temp is data packed at 279F. Then what is the temp that I have to PPAP to?
Hay, I am working on a paint project for steel driveshafts. The question is if the part sees a 300F oven for 17 minutes, and the part temp is data packed at 279F. Then what is the temp that I have to PPAP to?