Hi,
Can someone help me with this?
I am researching on fibrous concrete using steel fibres from recycled tyre. However, the steel fibes I am supplied with, are bundled in a chunk like a steel wool. (Not woven, but not seperate neither). I need to draw this chunk into separate steel fibres so that they do not ball in the mixer. Is there a mecchanical way how I can do this?
tks
Can someone help me with this?
I am researching on fibrous concrete using steel fibres from recycled tyre. However, the steel fibes I am supplied with, are bundled in a chunk like a steel wool. (Not woven, but not seperate neither). I need to draw this chunk into separate steel fibres so that they do not ball in the mixer. Is there a mecchanical way how I can do this?
tks