Ingenuity

Structural
May 17, 2001
2,374
Has any one used or have experience with this DRADER INJECTIWELD plastic welding unit?

Link

My application is 2.0mm thick HDPE tubing of 16mm diamater where I wish to weld a longitudinal seam.


 
Replies continue below

Recommended for you

You might consider sending them a sample and asking them to perform a weld on it to demonstrate their machine's capability.

It is better to have enough ideas for some of them to be wrong, than to be always right by having no ideas at all.
 
Thanks, ornerynorsk, excellent idea. Star for you!
 
By way of follow-up, I sent a sample to one of the manufacturer's resellers and they conducted a trial weld and returned the sample to me:

image_qomlpj.jpg
 