GonzaloMartinez
Mechanical
Hello everyone,
I would like to hear (read) your thoughts on the image I'm posting. It belongs to a 4140, 2" diameter steel bar . Notice the coarse acicular structure + fine pearlite grains (?). I was told by a material specialist that it corresponds to the absence of heat treatment after rolling (uncontrolled cooling) but I could not find any similar image in the bibliography to support it. Do you agree with that statement?
Best Regards,
Gonzalo M.
Magnification 100X
I would like to hear (read) your thoughts on the image I'm posting. It belongs to a 4140, 2" diameter steel bar . Notice the coarse acicular structure + fine pearlite grains (?). I was told by a material specialist that it corresponds to the absence of heat treatment after rolling (uncontrolled cooling) but I could not find any similar image in the bibliography to support it. Do you agree with that statement?
Best Regards,
Gonzalo M.
Magnification 100X