Hi All,
I am working on a Pipeline project in Canada, where our Contractor has developed WPS based on wire-fed processes (GMAW and FCAW) for produced emulsion, gas and steam pipelines and wants to conduct Radiography (RT) to detect imperfections. The owner fears that radiography is not an appropriate technique for detecting imperfections that are inherent to wire-fed processes and proposed to use Phased Array technique (PA-UT)instead. Contractor is adamant on using the radiography as they already developed welding procedures and welders are qualified. Contractor thinks that it is too late for the contract. Now owner is saying that they will do PA-UT on their cost and if there is a defect identified then Contractor will have to repair it. Of course Contractor is not agreeing to that also as they think that it is unfair to use combination of two NDE techniques.
Now I have two questions:
1. based on your experience/understanding do you that RT is not appropriate for these kinds of welding processes? if so, why?
2. Does owner have the right to perform PAUT and ask contractor to fix it, if unacceptable indication is found?
I am working on a Pipeline project in Canada, where our Contractor has developed WPS based on wire-fed processes (GMAW and FCAW) for produced emulsion, gas and steam pipelines and wants to conduct Radiography (RT) to detect imperfections. The owner fears that radiography is not an appropriate technique for detecting imperfections that are inherent to wire-fed processes and proposed to use Phased Array technique (PA-UT)instead. Contractor is adamant on using the radiography as they already developed welding procedures and welders are qualified. Contractor thinks that it is too late for the contract. Now owner is saying that they will do PA-UT on their cost and if there is a defect identified then Contractor will have to repair it. Of course Contractor is not agreeing to that also as they think that it is unfair to use combination of two NDE techniques.
Now I have two questions:
1. based on your experience/understanding do you that RT is not appropriate for these kinds of welding processes? if so, why?
2. Does owner have the right to perform PAUT and ask contractor to fix it, if unacceptable indication is found?