Does a PQR for FCAW and a PQR for GTAW qualify a WPS for FCAW / GTAW

Status
Not open for further replies.

thefreodockers

Mechanical
Jan 30, 2007
6
As the title states:

Does a PQR for FCAW and a PQR for GTAW qualify a dual process WPS for FCAW / GTAW?
 
Replies continue below

Recommended for you

You mean a combined, not dual, process procedure? Yes.
 
If possible, for future reference, could you point me in the right direction to finding this out myself?
 
Yes.
ASME Boiler and Pressure Vessel Code, Section IX, Article 2.
 