Doeconcreting onto or forming a slope

Status
Not open for further replies.

ukengineer58

Civil/Environmental
Oct 28, 2010
182
does anyone have any references or information on slump/consistency of concrete for casting to a or on a slope. For instance for a slope of > x degrees do you reduce the slump maybe?
 
Replies continue below

Recommended for you

We have successfully placed 3" slump concrete on 1.5:1 slopes at a 4" thickness. Slopes lengths were less than 23' or so.
 
See attached thread. It doesn't answer your question specifically but it may help.

thread507-252752
 