DOD-L-85645A1 LUBRICANT, DRY FILM, MOLECULAR BONDED was inactivated on 1994 and 2000 for new designs. Is there a new process to replace it? Does anyone has an idea for the reason/s it was inactivated for new designs?
 
Replies continue below

Recommended for you

Hello. The person/company who can answer your question is:

Charles J Beall
Division Manager Everlube Products
MIC Group Technical Director
A Curtiss-Wright Corporation Business Segment
Phone:(770) 261-4821
Fax: (770) 261-4859
e-mail: Charles_Beall@everlubeproducts.com
Charles_Beall@metalimprovement.com





William Gunnar
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor