Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Documents Required to be Submitted by the vendor for Bulk Components Piping / Flanges / Fittings

Status
Not open for further replies.

myck

Mechanical
Joined
Nov 26, 2013
Messages
13
Location
PH
Dear All,

Looking for Help. I am reviewing Bid from different Piping Component Vendor. I am not sure what documents shall they submit to us after Purchase. I think Material Certificate is enough. Can anybody tell significant document aside from Matl. Cert.

Regards,
Myk
 
What documentation did the invitation to bid package specify?

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 
And what is written in your purchasing requirements?
Many people require additional documents, such as chemistry certs from the original melter, and NDT reports if applicable.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
Yes Sir. There are document requirement. But i believe that not all are needed and i am not sure which should i accept. A pipe supplier may provide a mill cert ( usually contains all necessary test for component from a mill including chemistry). Anyway if you have experience aside from mill cert please let me know for reference. Thanks a lot.
 
Dear Myck,

1. Mill Certificate / MTC

2. NDT reports

3. 3rd party inspection reports

4. PMI reports (as 1. may not be available)

Regards.

DHURJATI SEN
 
Add the dimension drawing to the required document list above. Also, make sure the bidder proposal commit to the required documents dates as specified on PO.
 