Hello All,
is anyone familiar with DNVDNVGL-ST-F101 . I need your assistane on NDT Acceptance Criteria?

Could anyone explain me RT acceptance criteria for cluster porosity??

Welded material is CS with 20mm wall thickness.

DNVGL-ST-F101 2017



Regards
Ilkin HASANOV
 
 https://files.engineering.com/getfile.aspx?folder=cfd8aade-3657-432d-9f50-b6e17a3bf718&file=DNV_NDT_.png