Dissimilar welding of p1 to P8 materials for a pressure vessel (ASME VIII div.1), plate thickness is 40mm.
(1) If materials are used for pressure parts, what is the preheat temperature I can use? Can I do PWHT for them?
(2) If materials are used for Non-pressure part, what is the preheat temperature I can use? Is PWHT required by code?
ASME VIII div.1 is used for the pressure vessel construction.
Please advise. Thanks.