Hello,
As Per QW 423.1 When a base metal shown in the left column is used for welder qualification, the welder is qualified to weld all combinations of base metals shown in the right column, including unassigned metals of similar chemical composition to these metals.
Does it mean any combination like, if base metal in welder qualification is P1-P1 GTAW+SMAW with or without backing with F.no 6 & 5 then he is qualified to weld P1-P8 GTAW+SMAW with or without backing with F.no 6 & 5 ?
As Per QW 423.1 When a base metal shown in the left column is used for welder qualification, the welder is qualified to weld all combinations of base metals shown in the right column, including unassigned metals of similar chemical composition to these metals.
Does it mean any combination like, if base metal in welder qualification is P1-P1 GTAW+SMAW with or without backing with F.no 6 & 5 then he is qualified to weld P1-P8 GTAW+SMAW with or without backing with F.no 6 & 5 ?