Hi,
We need to make a tool that has a very small opening when
finished, it needs to be made over a male mandrel.
I'd like to know if anyone has played with Wax or Casting Metals to acheive this ? Maybe Sand with a expandable bladder ?
We have to be able to remove the mandrel after the part is cured.
Any suggestions ?
Thanks !