We need to make a tool that has a very small opening when
finished, it needs to be made over a male mandrel.

I'd like to know if anyone has played with Wax or Casting Metals to acheive this ? Maybe Sand with a expandable bladder ?

We have to be able to remove the mandrel after the part is cured.

Any suggestions ?

Thanks !
 
There are a number of materials available to make tooling that is soluble in water or other media.

google "soluble tooling" and there are 42000 hits.

good luck

Composites and Airplanes - what was I thinking?

There are gremlins in the autoclave!
 
ive used axpandable silicone bladders over a low melt alloy core it works really well
 
I have use extruded styrofoam, and then melt it with acetone or gasoline, but a good result depends on what size a piece you are making.

another way I do it, first a waxed balsa plug, then a thin layer of glass and epoxy, when split open this shell, take the wood out, glue it back together, and laminate over this shell.

contact me if you want to talk more about this, I don´t check eng tips too often.
 
make sure that the temperture you need to melt is above your cure temp and below the working limit of the material.
 