So a fabricator made a PQR based on these parameters:
T = 50 mm
GTAW t (root) = 8 mm
SMAW t (middle passes) = 21 mm
SAW t (subsequent passes plus cap) = 21 mm
The PQR above is used to support a WPS with SMAW only and T and t ranges of 8 mm to 200 mm. (The WPS stated backing is required but this point is moot in this discussion.)
I don't see any problem with this and my opinion is that this in compliance of the Code.
Thoughts, anyone?
T = 50 mm
GTAW t (root) = 8 mm
SMAW t (middle passes) = 21 mm
SAW t (subsequent passes plus cap) = 21 mm
The PQR above is used to support a WPS with SMAW only and T and t ranges of 8 mm to 200 mm. (The WPS stated backing is required but this point is moot in this discussion.)
I don't see any problem with this and my opinion is that this in compliance of the Code.
Thoughts, anyone?